HEMA and PPG Enable Simultaneous Control of Overcuring and Debinding Defects in Photopolymerizable β-Tricalcium Phosphate Ceramic Printing Slurries
Ceramic parts fabricated by vat photopolymerization often suffer from pores, delamination, and cracks, which greatly limit their development, mainly due to poor slurry flowability, high polymerization shrinkage stress of the resin, and insufficient removal of organics. To address the above challenges, this study inve...