Study on the Performance Degradation and Three-Dimensional Pore Structure Evolution of Synchronous Grouting Material for Subsea Shield Tunnels Under Long-Term Natural Seawater Corrosion
Sep 2026· Journal of Marine Science and Engineering· Vol 14, pp. 1626· 0 citations· 34 references
Abstract
The synchronous grouting layer in subsea shield tunnels is continuously exposed to seawater during long-term service. Sustained migration and diffusion of seawater ions can induce deterioration of the pore structure and degradation of mechanical properties, thereby diminishing the support and load-transfer functions provided to the segmental lining and ultimately compromising the long-term structural safety of the tunnel. In this study, synchronous grouting mortar obtained from an actual subsea shield tunnel project was subjected to freshwater and natural seawater immersion. Compressive strength tests and X-ray computed tomography were combined to investigate the evolution of mechanical properties and three-dimensional pore structure under prolonged exposure to natural seawater. Repeated scans were performed on the same group of samples at different immersion ages to determine total porosity, connected porosity, and pore connectivity. Quantitative relationships were then established between immersion time and both connected porosity and compressive strength. The results indicate that natural seawater exerts a pronounced influence on compressive strength at different stages, shifting from an initial enhancement to progressive deterioration during prolonged immersion. At 420 d, the compressive strength was approximately 23% lower than the peak value measured at 28 d. During prolonged immersion, total porosity increased gradually, whereas connected porosity and pore connectivity exhibited substantial increases. The difference shows that the internal structural evolution was governed primarily by the propagation and interconnection of existing pores and microcracks rather than by a substantial increase in total pore volume. With increasing immersion time, the pore structure progressively evolved from a dispersed and weakly connected state into a more continuous network of pores and cracks, accompanied by the enlargement and interconnection of local defects. The evolution of connected porosity with immersion time was well described by a square root function based on the characteristic time scale of Fickian diffusion, while the variation in compressive strength followed an exponential relationship. Increased connectivity of pores and cracks provided more continuous pathways for the inward transport of seawater ions and progressively disrupted the internal load-bearing framework, thereby contributing to the degradation of macroscopic mechanical properties. The findings provide experimental support for the durability design of synchronous grouting materials and the long-term maintenance of subsea shield tunnels.
Reinforced concrete structures in marine environments deteriorate over time due to the hydrodynamic effects of seawater exposure and the transport of salt-laden, humid air. In particular, fluid-driven permeation and diffusion of chloride and sulfate ions into the porous matrix lead to chemical reactions that cause rein...
M. Altun, Yusuf Çetinkaya, M. Durgun et al.· Turkish Journal of Civil Eng...· 0 citations
Long-term sealing performance of a CO2 injection well depends strongly on the mechanical integrity of the cement sheath and its bonds with the casing and formation. This study develops a static, three-layer thermo-poroelastic analytical screening model to evaluate prescribed pressure-increase and uniform-cooling end st...
K. Phuc, Vinh Bui, L. Nam et al.· IOP Conference Series: Earth...· 0 citations
Transpiration cooling through sintered metallic porous media is a promising active thermal-protection strategy for high-heat-flux aerospace and propulsion applications, yet the relative influence of the solid material, the pore architecture, and the pore diameter on cooling performance has not been established within...
Md Tarif Raihan, Ryoichi S. Amano· Journal of Energy Resources...· 0 citations
Concrete structures buried in saline soil environments are concealed and difficult to monitor. Sulfate-resistant cement has been widely used in early sulfate corrosion environments, yet an objective evaluation of its performance under real-world conditions remains urgently needed. In this study, test piles of ordin...
Xiao-Ping Wang, Rong-Ling Zhang, Qi-Cai Wang et al.· Journal of materials in civi...· 0 citations
Austenitic–ferritic stainless steels are frequently selected for components in seawater-cooling pumps in power plants and nuclear stations due to their generally superior resistance to localized and stress corrosion cracking (SCC) in comparison with austenitic grades. However, during operation, these cast components ar...
Imededdine Trigui, B. Louhichi, M. Terres· Corrosion and Materials Degr...· 0 citations
Hydro-mechanical coupling governs the stability of tunnel surrounding rock in soft-rock strata. Mudstone-type soft rocks exhibit abrupt strength loss and time-dependent large deformation under groundwater infiltration, posing severe threats to construction safety and long-term service performance. Most existing studies...
Hua-Chao Li, Qing-Song Su, Jian Yao et al.· Geotechnics· 0 citations