merrypopins: A Python package for nanoindentation data science

Oct 2026 · The Journal of Open Source Software · 15 references
Metal and Thin Film Mechanics

Abstract

merrypopins is a Python library that streamlines nanoindentation data processing, automated pop-in detection, and statistical analysis of collections of pop-in events.Nanoindentation deforms materials experimentally to characterise their behaviour and quantify mechanical properties from load-displacement data (Oliver & Pharr, 1992, 2004).Experiments performed with a spherical tip can also be used to construct stress-strain curves and, by extension, determine the yield point, defining the transition from elastic to plastic deformation (Kalidindi & Pathak, 2008;Pathak & Kalidindi, 2015).Understanding the onset of plasticity at the microscale matters for applications in engineered materials and earthquake mechanics.A common feature during the loading part of these experiments is a sudden increase of indentation depth at constant force, called a "pop-in".Recognising pop-ins by hand is labour-intensive and subjective, which makes automated, reproducible detection important.

Read PDF

Similar papers

#computer vision Review Sep 2017

Agile Software Development Methods: Review and Analysis

This publication proposes a definition and a classification of agile software development approaches and analyses ten software development methods that can be characterized as being "agile" against the defined criterion.

P. Abrahamsson, O. Salo, Jussi Ronkainen et al. · 727 citations · ⚡54
#computer vision Jun 2008

The impact of agile practices on communication in software development

The study shows that agile practices improve both informal and formal communication, but indicates that, in larger development situations involving multiple external stakeholders, a mismatch of adequate communication mechanisms can sometimes even hinder the communication.

M. Pikkarainen, Jukka Haikara, O. Salo et al. · 401 citations · ⚡48
#machine learning Review Open access Oct 2014

Software development in startup companies: A systematic mapping study

The results indicate that software engineering work practices are chosen opportunistically, adapted and configured to provide value under the constrains imposed by the startup context.

Nicolò Paternoster, Carmine Giardino, M. Unterkalmsteiner et al. · 394 citations · ⚡54

Trajectory Balance: Improved Credit Assignment in GFlowNets

It is proved that any global minimizer of the trajectory balance objective can define a policy that samples exactly from the target distribution, and empirically demonstrate the benefits of the trajectories balance objective for GFlowNet convergence, diversity of generated samples, and robustness to long action sequenc...

Esmeralda S. Whitammer, Moksh Jain, Emmanuel Bengio et al. · 302 citations · ⚡60

Related blog posts

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.