Physically guided SCAPS-1D analysis of ITO/CdS/Sb2Se3/Mo thin-film solar cells: back-contact energetics, thickness effects, and defect-mediated recombination

Sep 2026 · Physica Scripta · Vol 101 · 0 citations · 35 references
Physics

Abstract

Antimony selenide (Sb2Se3) is a promising absorber for thin-film photovoltaics because of its suitable band gap, strong optical absorption, simple binary composition, and comparatively low toxicity. In this work, a physics-guided SCAPS-1D analysis of a minimal ITO/CdS/Sb2Se3/Mo solar-cell architecture was performed to distinguish the influence of rear-contact energetics, layer thicknesses, bulk and interface defects, absorber doping, and selected parameter interactions. The Mo-based reference device yielded Voc = 0.7094 V, Jsc = 41.53 mA cm−2, FF = 82.73%, and PCE = 24.37% under AM1.5G illumination at 300 K. Rear-contact work-function analysis showed that low-work-function contacts strongly limit hole extraction and photovoltage, whereas Mo (Φm ≈4.95 eV) approaches a nearly non-blocking hole-contact condition within the idealized contact model. Increasing the Sb2Se3 thickness mainly enhanced Jsc below approximately 1.0 µm, whereas CdS thickness produced only minor changes over 0.02–0.20 µm. A low-bulk-defect plateau was identified between approximately 1010 and 1013 cm−3, while Nt,bulk approaching 1015 cm−3 enhanced distributed Shockley–Read–Hall recombination and degraded performance. Increasing Nt,int from 1010 to 1014 cm−2 reduced Voc from 0.7094 to 0.6050 V and PCE from 24.37% to 20.50%, while Jsc remained comparatively insensitive. Interface states located approximately 0.3–0.6 eV above the highest valence-band edge produced the strongest losses, consistent with the calculated interface recombination current. The isolated acceptor-concentration sweep identified NA ≈1016 cm−3 as a favorable balance between junction electrostatics and carrier collection, while a limited, targeted two-factor interaction assessment revealed coupling between absorber thickness and bulk defects and between doping and rear-contact energetics. Comparison with recent experimental and numerical studies indicates that the 24.37% baseline represents an idealized numerical operating condition rather than a directly achievable efficiency. These results identify rear-contact selectivity, bulk-defect control, and CdS/Sb2Se3 interface quality as key targets for further device development.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.