Skip to content
Open access

Silicon Carbide Reinforced Bio-based Alkyd–Polyurethane Coatings: Structure–Property Relationship and Enhanced Barrier Performance

Sep 2026 · Journal of Polymers and the Environment · Vol 34 · 0 citations · 47 references

Abstract

The transition away from petroleum-derived coatings requires bio-based systems that match the durability of their fossil counterparts without compromising renewable content. In this work, polyurethane (PU) nanocomposite coatings were developed from Niger seed oil (NSO), an underutilized non-edible vegetable oil, and bio-derived itaconic acid, with silicon carbide (SiC) nanoparticles incorporated at 1, 3, and 5 wt% as reinforcement. The Niger seed oil-based monoglyceride and alkyd resin were characterized by proton nuclear magnetic resonance (1H-NMR) and Fourier-transform infrared spectroscopy (FT-IR), with quantitative ¹H NMR integration confirming ≈ 92% conversion of triglyceride to monoglyceride. Scanning electron microscopy (SEM) and atomic force microscopy (AFM) revealed uniform near-surface SiC dispersion, with the arithmetic-mean roughness rising progressively from 0.29 nm for the neat coating to 0.87 nm at 5 wt% SiC, while X-ray diffraction (XRD) revealed an increasing apparent composite crystalline fraction with increasing nanoparticle content. Crosslinking density was assessed through gel content and independently validated by Flory–Rehner swelling analysis, yielding νₑ values of 0.42 to 1.18 × 10− 3 mol cm− 3, while differential scanning calorimetry (DSC) showed a monotonic rise in glass transition temperature from 58 °C (NSOPU-0) to 85 °C (NSOPU-5), confirming progressive network densification. Incorporation of 5 wt% SiC (NSOPU-5) delivered a 41% increase in tensile strength, 191% improvement in abrasion resistance, 26% reduction in water uptake, a water contact angle of 113.3°, a charge-transfer resistance (Rct), measured by electrochemical impedance spectroscopy (EIS), of 1.1 × 107 Ω·cm2, and a char residue of 30.9% at 700 °C. The cured coatings exhibit a calculated bio-based carbon content of 74.2% under the United States Department of Agriculture (USDA) convention, against 0% for a fully petroleum-derived two-component PU reference, and achieve protective performance competitive with a previously reported petroleum-based PU benchmark. The combination of a non-edible vegetable oil, a fermentation-derived dicarboxylic acid, and ceramic SiC reinforcement establishes Niger seed oil/itaconic acid/SiC nanocomposites as promising renewable candidates for protective coating applications, offering a route toward reducing reliance on fossil-derived feedstocks.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.