The growing demand for Portland cement has intensified concerns over construction-related CO2 emissions, driving interest in low-carbon alternatives such as alkali-activated concrete (AAC). Although AAC can substantially reduce embodied carbon, the production of commercial sodium silicate (SS), a widely used activator, remains a significant environmental burden. This study evaluates the feasibility of a waste-derived sodium silicate activator produced from silica fume (SF) and sodium hydroxide (NaOH) and compares its performance with that of a conventional commercial activator in blended f fuel ash (PFA) and ground granulated blast furnace slag (GGBS) systems. Fresh and hardened properties were assessed across a range of activator-to-binder (A/B) and SS/SH ratios, considering workability, setting time, and compressive strength requirements for structural concrete applications. Increasing the A/B ratio from 0.16 to 0.20 improved compressive strength and accelerated setting, while higher SS/SH ratios enhanced early- and later-age strength through increased soluble silica availability and gel formation. Although higher activator contents reduced workability due to increased viscosity, both commercial and SF-derived activators achieved comparable mechanical performance. The high amorphous silica content of SF was found to promote dense C-(A)-S-H gel development, while 10 M NaOH and a 24 h ambient-temperature extraction process provided sufficient silica dissolution without additional heating. These findings demonstrate the potential of SF-derived sodium silicate as a sustainable activator for producing low-carbon AAC with performance comparable to conventional systems.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.