Cooling-path dependence of crystallographic texture in L10-FePt thin films derived from Fe/Pt multilayers
Abstract
The cooling stage of postdeposition annealing is often regarded as a passive step that preserves the structure formed at high temperature. Herein, we examined whether the cooling path affects the crystallographic texture of L10-FePt films derived from Fe/Pt multilayers on thermally oxidized Si(100). After a 240 min hold at 700 °C, specimens were cooled either at different nominal rates or using a switching protocol in which controlled cooling at −1 °C min−1 was terminated at a switching temperature Tsw, followed by natural cooling. Changing the nominal rate altered the preferred texture from (111)-dominant to (001)-enhanced. Extending controlled cooling to 200 °C rather than 450 °C increased the relative (001) diffraction contribution and narrowed the (001) rocking curve. The accompanying increase in out-of-plane loop squareness was qualitatively consistent with this structural trend. These results establish the cooling stage as an active process parameter for controlling the final L10-FePt texture.