The effect of post weld heat treatment (PWHT) on the mechanical properties (joint toughness) of friction stir weld joints of AA7000 using tool material of carbide tungsten (WC)
Abstract
AA7075-T651 aluminum alloy is indispensable for weight-critical aerospace and automotive structures due to its exceptional strength-to-weight ratio, yet its weldability remains challenging via conventional fusion techniques. Friction stir welding (FSW) with a tungsten carbide (WC) tool offers a solid-state alternative that minimizes defects but induces microstructural degradation—particularly dissolution of strengthening precipitates and grain boundary alterations—severely reducing joint toughness, especially in the nugget zone (NZ). This work implemented post-weld heat treatment (PWHT) to restore precipitate distribution, systematically evaluating T6 (peak aging) and T7 (overaging) cycles on AA7075 FSW joints. Welding employed a WC tool (18 mm shoulder, 7.2 mm pin) at 800 RPM/90 mm/min. PWHT included solution treatment (480 °C/1 h) followed by T6 (120 °C/24 h) or T7 (105 °C/8 h + 170 °C/16 h) aging. Mechanical and microstructural characterization included Vickers hardness mapping, tensile testing (ASTM E8), Charpy V-notch impact tests (ASTM E23) with NZ-notched specimens, and OM/SEM fractography. Results indicated that T6 restored 94% of base metal tensile strength (538 MPa) but achieved only modest toughness (12.1 J). T7, however, tripled NZ impact energy (21.5 J) versus the as-welded state (7.2 J) by coarsening intragranular η-phase precipitates (115 nm), reducing grain boundary precipitate density by 52% (1.2 μm⁻¹), and narrowing PFZs to 45 nm. Fractography confirmed fully ductile fracture in T7 specimens, contrasting with brittle intergranular failure in T6. The T7 cycle is identified as optimal for NZ toughness enhancement, providing manufacturers a pathway to improve impact resistance in safety-critical FSW AA7000 applications.