Oct 2026· ACS Applied Polymer Materials· 0 citations· 70 references
Abstract
The development of sustainable elastomeric materials is an important step toward reducing the environmental impact of conventional synthetic rubbers. In this study, elastomeric electrospun materials were fabricated from blends of amorphous polyhydroxyalkanoate (aPHA) and cellulose acetate (CA) at three compositions (50/50, 75/25, and 90/10). The influence of fiber morphology and interfiber bonding on the mechanical response was investigated. Neat aPHA showed rubber-like behavior but poor dimensional stability after electrospinning. Incorporating CA improved structural stability, thermal resistance, tensile strength, and Young’s modulus. The 90/10 (aPHA/CA) blend retained a hyperelastic response, consistent with the classical Ogden and Mooney–Rivlin strain-energy models, while improving processability. Morphological analysis during stretching–relaxation cycles revealed a bimodal fiber diameter distribution, originating from axial fiber thinning and perpendicular fiber compression due to interfiber fusion points. A permanent diameter increase of perpendicular fibers (∼20%) was observed after the first cycle and stabilized upon repeated deformation. Fitting of uniaxial stress–strain data to Ogden and Mooney–Rivlin functions confirmed that pure aPHA and the 90/10 blend possess rubber-like properties, whereas the 75/25 composition did not. The biodegradation analysis supports the sustainable nature of the developed rubber-like materials, with all blends exhibiting full biodegradation in compost within 37 days. These results show that controlled CA incorporation regulates interfiber bonding and structural stability, enabling the design of fully biobased electrospun elastomeric materials.
High-density polyethylene (PE) plays a central role in polymer composite materials due to its excellent mechanical properties, ease of processing, and low cost. In the quest for more sustainable materials, biosourced fillers like microgranular cellulose (MGC) have emerged as a promising alternative to conventional re...
Brieuc Le Besnerais, Licia Gaeta, Nathan J. Van Zee et al.· ACS Applied Polymer Material...· 0 citations
This study investigates the incorporation of cellulose as a bio-based modifier into polyurethane foam and its effects on molecular interactions, morphology, thermal behavior, and mechanical performance. Polyurethane foam was synthesized using polypropylene glycol (PPG 2000), toluene diisocyanate (TDI), water, and cellu...
Rina Ningtyas, Muhammad Emirsyah Putra, Dea Talitha Syahara et al.· Indonesian Journal of Chemis...· 0 citations
Polylactide (PLA)-based foams are viable sustainable alternatives to traditional petroleum-derived foams owing to their intrinsic biodegradability, superior biocompatibility, light weight, and high specific strength, with potential applications in packaging, insulation, and biomedical fields. However, their inherently...
Silla George Raju, Valentina Volpe, Rita Salomone et al.· Industrial & Engineering Che...· 0 citations
Electrospun fibers of polyhydroxyalkanoate (PHA), blended with PCL or PBS, were loaded with linezolid (LIN) to investigate induced morphological evolution, crystallization, and strain-induced deformation micromechanics. Up to the optimal nucleating concentration of 2 wt %, LIN was fully encapsulated, increasing PCL cry...
R. Hosseinnezhad, Dhanumalayan Elumalai, Mehrnaz Khalaji· Biomacromolecules· 0 citations
Polydimethylsiloxane (PDMS) is a widely used silicone elastomer owing to its flexibility, chemical inertness, optical transparency, and biocompatibility. However, its relatively low mechanical strength, poor thermal and electrical conductivity, and hydrophobic surface limit its performance in advanced applications....
Ravinder Kaur, Karanbir Singh, R. Mehta· Journal of Applied Polymer S...· 0 citations