Experimental study on the flexural behavior of precast jointed slabs with an ultra-thin UHPC layer

Oct 2026 · Journal of Physics, Conference Series · Vol 3336 · 0 citations · 13 references
Physics

Abstract

Four-point bending tests were carried out on four representative specimens of precast jointed slabs incorporating an ultra-thin UHPC (Ultra-High Performance Concrete) layer to assess their flexural behavior. Comparative analyses were conducted on the failure modes, load-deflection responses, strain distributions, and crack propagation characteristics of straight-bar joints, looped-bar joints, and steel–UHPC composite joints. The results indicate that cracking in all specimens initiated near the joint interface, confirming that the joint region is the critical weak zone governing flexural performance. The straight-bar joint specimens exhibited a cracking load of 4 kN and an ultimate load of 23 kN, with cracks developing quickly and the overall response showing clear brittle characteristics. For the looped-bar joint specimens, the cracking load increased to 6 kN, and the ultimate load increased to 34-35 kN. Moreover, the cracks were more uniformly distributed, and the post-cracking stiffness retention was improved, while the overall flexural performance showed little difference between the two bending directions of the bars. For the steel–UHPC composite joint specimens, the cracking load further increased to 12 kN, and the ultimate load reached 63 kN, representing a substantial improvement over the straight-bar joint specimens. In addition, the development of reinforcement strain, UHPC tensile strain, and crack width in the joint region was effectively restrained, demonstrating superior crack resistance and composite action.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.