Skip to content

Two distinct interface structures and fracture behavior in oscillating laser welding of Al/Mg dissimilar metals

Oct 2026 · Science and technology of welding and joining · 0 citations · 35 references

Abstract

In this study, high-frequency circular oscillating laser is employed to achieve a more uniform energy distribution and a Ti interlayer is used to suppress the continuous and excessive formation of brittle Al–Mg intermetallic compounds (IMCs). The results show that the joint interface exhibits an optimal “U-shaped” morphology at 3.0 kW with the Ti interlayer melting uniformly. The interface is primarily composed of a 6-μm Al–Mg IMCs layer and a 23-μm Al–Ti IMCs layer. During shear tests, fracture occurs along the Al–Ti IMCs layer. At 3.5 kW, the Ti interlayer is completely penetrated, and the interface transforms into an “n-shaped” configuration consisting of an α-Mg + Al 12 Mg 17 eutectic phase and a dispersed mixture of Al–Ti IMCs. Fracture occurs at the Mg-side fusion line. Neither joint exhibits large-area, single-phase Al–Mg IMCs. Instead of occurring at the conventional Al–Mg interface, fracture is shifted to the Mg-side fusion line, allowing both joints to achieve reliable strengths of ≥2.5 kN.

View source

Similar papers

Oct 2026

Dissimilar joining of 6061 Al alloy and FeCoNiCrMn HEA by CMT arc welding-brazing: Microstructure and interfacial behaviour

6061 Al alloy was joined to FeCoNiCrMn high-entropy alloy by Cold Metal Transfer advanced arc welding-brazing with an Al filler. Increasing heat input from 55 to 139 J mm −1 improved wetting, increasing the wetting length from ∼1.8 to ∼4.6 mm and decreasing the wetting angle from ∼140° to ∼70°. A continuous bilayer...

Gao-Yang Yu, Xiao-Ming Nie, Jin-Chao Xu et al. · 0 citations
Nov 2026

Interfacial reaction modification in Al/steel joints using a Si-rich interlayer during wire-based friction stir additive manufacturing

Joining low-Si 5B06 Al alloy to steel is limited by brittle Fe-Al intermetallic compounds. Here, a Si-rich 4043 Al interlayer (4.5 wt.% Si) was locally introduced between 5B06 Al alloy (0.24 wt.% Si) and 316L stainless steel during wire-based friction stir additive manufacturing. Compared with a direct 5B06/316L join...

Jin-Qi Wang, Xiang-Chen Meng, Yi-Fan Zhang et al. · 0 citations
Open access Oct 2026

Development of New Al-Ca-Cu-Mn-Zr Alloys for Laser Powder Bed Fusion

The limited thermal stability of conventional aluminium alloys at elevated temperatures restricts their application in laser powder bed fusion (LPBF). In this study, a novel Al6Ca3Cu1.8Mn0.4Zr (wt.%) alloy was developed for improved thermal stability via stable intermetallic phases. LPBF processing of gas-atomised powd...

S. Cherkasov, N. Letyagin, P. A. Palkin et al. · 0 citations
Open access Oct 2026

Thermal Input-Driven Interfacial Phase Evolution and Mechanical Reliability of Zn-15Al Brazed Cu/Al Joints

The effects of brazing temperature and holding time on the interfacial evolution and shear strength of Cu/Zn-15Al/Al joints were investigated. Joints were prepared at 480–540 °C for 1–9 min and characterized by SEM, EDS, shear testing and response-surface analysis. At low thermal input, an Al4.2Cu3.2Zn0.7-rich structur...

Tao Chen, Peng He, Teng-Zhou Xu et al. · 0 citations
Open access Nov 2026

Joining of Al 5052 Alloy to Advanced High-Strength Steel Sheets of Dissimilar Thickness Using Laser-Assisted Friction Stir Welding

Multi-material mixed structures (MMMS) are becoming increasingly important to meet the demand for lightweighting in the automotive industry. In this study, the joining of 2.5 mm thick Al 5052 alloy and 1.4 mm thick DP 590 steel sheets was conducted using laser-assisted friction stir welding (LAFSW). A parametric study...

Kyounghak Kim, Hee-Seon Bang · 0 citations