Low-temperature growth of high-quality Bi2O2Se for high-performance photodetection
Abstract
Bi2O2Se is a high-mobility, narrow-bandgap n-type layered semiconductor promising for broadband photodetection. However, its synthesis often relies on high temperatures or complex precursor systems that increase the thermal budget and limit device integration. Here we report a low-melting-point precursor-assisted chemical vapor deposition (CVD) strategy for growing high-quality Bi2O2Se nanosheets at 450 °C. Using elemental Bi and Se powders under an Ar/O2 atmosphere, we obtain single-crystalline nanosheets with uniform composition, long-term air stability and lateral sizes up to 0.6 mm. Photodetectors fabricated from the nanosheets show broadband response from 520 to 1550 nm, with a responsivity of 14.17 A∙W−1 and a specific detectivity of 6.39 × 1010 Jones at 1550 nm. The devices also exhibit fast response, with rise and fall times of 59 and 67 μs, respectively. Single-pixel imaging at 520 and 1550 nm further demonstrates their visible and near-infrared imaging capability. This work establishes low-melting-point precursor-assisted CVD as an effective route for low-temperature Bi2O2Se growth and points to its potential in broadband, high-speed photodetection.