4Cr13 martensitic stainless steel is widely used for plastic molds, but welding repair can produce heterogeneous weld/HAZ microstructures and a strength–toughness trade-off. This study evaluates how filler-wire composition and post-weld heat treatment affect the mechanical performance of repaired 4Cr13 steel. TIG welding was performed using high-molybdenum (HM), low-carbon (LC), and base-metal (BM) wires, followed by either post-weld tempering or quenching and tempering. Post-weld quenching and tempering reduced the hardness gradient and improved the overall hardness uniformity. The average weld-metal hardness followed HM > BM > LC, while the BM joint showed the smallest hardness variation because its nominal composition matched that of the base metal. After quenching and tempering, the tensile strengths of the HM, LC, and BM joints reached 1299.5, 1315.6, and 1300.0 MPa, respectively, compared with 1290.8 MPa for the similarly treated base metal. The corresponding impact energies were 58.9, 116.3, and 36.8 J, with LC showing the highest toughness. Fracture observations were consistent with these mechanical-property differences. The results demonstrate that filler-wire composition and post-weld heat-treatment route should be selected jointly according to the required balance of hardness uniformity, strength, ductility, and impact toughness, providing an experimental basis for repair-welding process selection for 4Cr13 steel.
Dissimilar welding of austenitic stainless steel and low alloy steel is widely employed in pressure vessels, petrochemical plants, power generation systems, and structural applications because it combines the corrosion resistance of stainless steel with the high strength of low alloy steel. However, acquiring high qual...
S. Noonari, A. Jamali, Q. Jamali et al.· Journal of the Serbian Chemi...· 0 citations
Dissimilar aluminium alloys are widely used in automotive and aerospace structures because they are lightweight and strong. However, joining these alloys by fusion welding remains challenging because their different chemical compositions and thermal behaviour strongly affect weld quality. This study investigates how jo...
Okoubulu Augustine B., Ajao Akeem M., Nwaeju-Okechukwu Cynthia C. et al.· European Journal of Material...· 0 citations
Hybrid lightweight structures increasingly combine cast, wrought, and additively manufactured aluminum alloys, but the mechanical response of their welded joints remains strongly material-dependent. In this study, cast EN AC-42100-T6, wrought EN AW-6082-T6, and laser powder bed fusion (LPBF) AlSi10Mg stress-relieved pl...
Omar Bologna, S. Cecchel, Riccardo Ferraresi et al.· Metals· 1 citation
Although Friction Stir Welding (FSW) reduces defects associated with conventional fusion welding of high-strength aluminium alloys such as AA7075 and AA2024, the resulting joints may still exhibit microstructural heterogeneity, residual stresses, and reduced joint efficiency. Limited studies have investigated cryogenic...
M. Fakhri· Journal of Mechanical Engine...· 0 citations
This study investigated the effects of filler metal composition and δ-ferrite characteristics on the cryogenic behavior and corrosion resistance of 316L austenitic stainless steel (STS) welds produced by gas tungsten arc welding (GTAW) using 309L and 312 filler metals (FMs). Different δ-ferrite fractions and morphologi...
Haneul Jeong, Hyunbin Nam, Y. Yoon et al.· Metals· 0 citations
The evolution of microstructure and mechanical properties in electrolytic tough-pitch (ETP) copper subjected to hybrid friction welding (HFW) was investigated. The effect of introducing a programmable brake on the flywheel’s rotation while maintaining constant friction and forging pressures was explored. The welded joi...
Michail Dellepiane, Laurie da Silva, A. Toumpis· Materials· 0 citations