Failure investigation and degradation study of long term hydrothermally stressed PVC reinforced with ZnO nanocomposites for cable insulation applications

Oct 2026 · Scientific Reports · Vol 16 · 0 citations · 35 references

Abstract

Water and temperature are critical environmental stresses that significantly affect the performance and longevity of insulation systems, particularly polymeric insulators. These factors lead to the degradation of the physical and chemical properties of polymers, ultimately resulting in failure. To investigate this, ZnO-based PVC nanocomposites (PZ0, PZ2, PZ4, and PZ6) were developed with varying concentrations of ZnO (0, 2, 4, and 6 phr). These nanocomposites were subjected to hydrothermal aging for 5000 h, divided into five cycles of 1000 h each, to assess their structural stability and performance over prolonged exposure to harsh conditions. Characterization of the nanocomposites was performed using techniques such as X-ray diffractometry (XRD), Fourier transform infrared (FTIR) spectroscopy, and scanning electron microscopy (SEM). The analyses revealed that the nanocomposites generally outperformed neat PVC in terms of structural integrity and resistance to aging. Notably, PZ2 exhibited the highest contact angle of 78° after the aging period, indicating improved hydrophobicity. Additionally, surface roughness measurements showed that PZ2 had significantly less roughness compared to the other composites, suggesting better durability and performance against environmental stresses. The FTIR analysis highlighted substantial degradation of the polymer structure, with all samples experiencing over 80% chain scission after 5000 h of aging. In particular, PZ4 demonstrated 56% and 86% degradation in specific absorption bands related to -CH2 stretching and C–C bending. Thermal stability was assessed using differential scanning calorimetry (DSC), which indicated that hydrothermal aging affected the melting points of the composites. Despite this, effective dispersion of the ZnO nanofiller within the polymer matrix provided enhanced stability, mitigating some adverse effects of aging. The failure analysis showed that PZ0 experienced 77% degradation after the first aging cycle, while PZ4, PZ0, and PZ6 exhibited 55%, 50%, and 66% degradation, respectively, underscoring the critical role of nanocomposite formulation in enhancing performance under environmental stress.

Read PDF

Similar papers

Open access Oct 2026

RSM-based optimization of mechanical and moisture resistance properties of ternary polymer nanocomposites

Epoxy-based polymer Nanocomposites are widely investigated for electrical insulation applications due to their exceptional mechanical and dielectric properties; however, moisture absorption and brittleness remain major challenges. This study aimed to develop and optimize Epoxy/ Ethylene Propylene Diene Monomer (EPDM)...

Aynamaw Betsene Wero, B. S. Yigezu · 0 citations
Oct 2026

Analysis of mechanical strength and corrosion resistance in AA6061-T6 aluminum alloy through optimized heat treatment

This work examines how heat-treatment parameters affect the mechanical properties, corrosion resistance, and fracture behavior of commercial AA6061 aluminum alloy. We used a Taguchi L 9 (3 4 ) orthogonal experimental design to evaluate the effects of solutionizing temperature (520–540 °C), solutionizing duration...

I. Guzmán-Flores, E. Granda-Gutiérrez, C. Cruz-González et al. · 0 citations
Open access Oct 2026

Processing of PVDF/Nb5+ and Sr2+-Doped PZT Composites for Applications in Advanced Dielectric Insulation: Effect of Ceramic Loading on Structure, Mechanical Properties, Electrical Properties, and Thermal Aging Behavior

In this study, four types of materials suitable for use as special insulation were produced. Polyvinylidene fluoride (PVDF) served as the polymer matrix, while PZT powders (a Pb(Zr0.52Ti0.48)O3 system doped with Nb5+ and Sr2+) were used as the filler material; the method for producing these powders is also described. T...

A. Caramitu, R. Ciobanu, A. Dumitru et al. · 0 citations
Open access Oct 2026

Investigation on the Electrical Breakdown Voltage Performance of LLDPE-Natural Fiber Composite Under Normal and Saltwater Immersion Conditions

The development of environmentally friendly insulating materials has attracted significant attention due to increasing environmental concerns associated with conventional petroleum-based polymers. This study investigates the dielectric performance of Linear Low-Density Polyethylene (LLDPE)–Natural Rubber (NR) composite...

Wan Muhammad Farish Wan Kamari, Nor Akmal Mohd Jamail, Q. E. Kamarudin · 0 citations
Open access Sep 2026

Epoxy reinforced with mesoporous hydrotalcite for high-voltage insulation application

Epoxy-based solid insulation is widely used in high-voltage systems; however, its breakdown reliability and thermal endurance remain critical limitations under coupled electrothermal stresses. This study investigates mesoporous Mg/Al hydrotalcite as a multifunctional nanofiller for enhancing the dielectric, breakdown,...

Mahmoud Ezzat, A. Said, Musa A. Said et al. · 0 citations
Open access Oct 2026

Investigation on the Degradation Mechanisms and Mechanical Property Evolution of 3D-SiO2-Fiber-Reinforced Polyimide Composites After Thermal Aging

Understanding the thermal aging behavior of SiO2f/PI composites is crucial for ensuring their reliability and longevity in high-temperature aerospace applications. In this study, the thermal aging behavior of three-dimensional quartz-fiber-reinforced polyimide (3D-SiO2f/PI) composites was investigated. The composites w...

Ming-Long Yang, Ya-Dan Wu, J. He et al. · 0 citations

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.