Skip to content

Analysis of transverse corner cracks and mould flux optimisation in the continuous casting of 34CrNiMo6 steel blooms

Oct 2026 · Ironmaking & Steelmaking: Processes, Products and Applications · 0 citations · 45 references

Abstract

34CrNiMo6 steel is widely used in heavy-duty transmission components, and improving its bloom surface quality is important for increasing product yield and reducing downstream processing costs. To address transverse corner cracking during continuous casting, mould flux evaluation, optimisation and industrial validation were conducted based on the steel's solidification characteristics, thermophysical properties and casting conditions. Calculations indicated a relatively low risk of peritectic transformation shrinkage, but low thermal conductivity increased corner shell sensitivity to non-uniform cooling and heat-flux fluctuations, demanding continuous liquid slag film lubrication and stable interfacial heat transfer. The existing Flux A exhibited a long melting time and high viscosity, break temperature and crystallisation temperature, resulting in a thin liquid slag layer and a shortened effective lubrication range that contributed to frequent cracking. Following the concept of ‘stable lubrication and controlled heat transfer’, Flux B was developed by reducing basicity, Al 2 O 3 and carbon contents, increasing Na 2 O content and introducing a small amount of Li 2 O. Optimisation reduced the melting temperature from 1185 °C to 1081 °C and the viscosity measured at 1300 °C from 0.59 to 0.36 Pa·s. Shorter melting time and lower break and crystallisation temperatures indicated improved melting and rheological properties and controlled high-temperature crystallisation. A parallel two-strand comparative trial over two consecutive heats showed that replacing Flux A with Flux B increased the liquid slag layer thickness from approximately 5 to 9 mm and mould flux consumption from 0.35 to 0.68 kg·t −1 . The number of transverse corner crack indications detected by magnetic particle inspection in the sampled blooms decreased from 20 to 3, representing a reduction of approximately 85%. These results demonstrate that mould flux optimisation based on steel solidification characteristics and thermophysical properties provides an effective approach to improving the bloom surface quality of Cr–Ni–Mo quenched-and-tempered steels.

View source

Similar papers

Open access Oct 2026

Regulation of Finishing Cooling Temperatures on Microstructure and Comprehensive Mechanical Properties of Microalloyed Weathering Steel in Thermo‐Mechanical Control Process

A Gleeble‐3500 thermo‐mechanical simulator was employed for this study. The effects of finishing cooling temperatures (450/500/550/600 °C) on the microstructural evolution and mechanical properties of a novel V–Ti–N microalloyed high‐heat‐input weathering steel were investigated. The results show that with the increase...

Bing-Li Hu, Wen-Bin Luo, Qiu-Ming Wang et al. · 0 citations
Sep 2026

Formation mechanism and control of surface peeling defect on a medium-carbon Cr–V system hot-rolled sheet

This work investigated the edge peeling defects observed in the hot-rolled sheets of a medium-carbon alloy spring steel (50CrV4). Combined experimental characterisation and numerical simulation were employed to elucidate the formation mechanism and control strategy of the defects. Optical microscopy and scanning electr...

Zhen-Dong Wang, Hai-Yan Tang, Lu Jin et al. · 0 citations
Conference Open access Oct 2026

Effects of the slag skin physical properties on the heat and mass transfer during initial solidification in continuous casting process

Initial shell formation in continuous casting is governed by coupled flow, heat transfer and mould-flux infiltration near the meniscus. In this work, an in-house two-phase OpenFOAM-based model with geometric VOF interface tracking is applied to study liquid-steel flow and solidification, slag infiltration and re-solidi...

Alexander Vakhrushev, E. Karimi-Sibaki, M. Wu et al. · 0 citations
Oct 2026

Multi‐Objective Optimisation of Surface Integrity and Energy Consumption in Ultrasonic‐Assisted Roller Burnishing of Al‐6082‐T6 Alloy Under MWCNT‐NMQL

Al‐6082‐T6 alloy is widely used in aerospace, automotive and defence industries due to its excellent durability, formability, corrosion resistance and high thermal conductivity. However, achieving high surface quality with sustainable manufacturing remains challenging. Roller burnishing, a chipless surface‐finishing...

Murat Yildiz, Prameet Vats, K. K. Gajrani et al. · 0 citations
Oct 2026

Tribological Performance of Pack Boronized AISI 4140 Steel via Waste‐Derived Green Lubricants at Elevated Temperatures

Enhancing the tribological performance of alloy steels under eco‐friendly lubrication and high‐temperature conditions has gained importance for sustainable engineering applications. In this regard, the current study investigates the impact of biolubricants and high temperatures on the tribological properties of AIS...

H. Ateş, Rahman Çalhan, Mehmet Tayyip Özdemir et al. · 0 citations

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.